Национальный цифровой ресурс Руконт - межотраслевая электронная библиотека (ЭБС) на базе технологии Контекстум (всего произведений: 636193)
Контекстум
Руконтекст антиплагиат система
Журнал Сибирского федерального университета. Химия. Journal of Siberian Federal University/ Chemistry  / №3 2015

Composition of Products of Birch Wood Deligniёcation by Hydrogen Peroxide in the Medium “Acetic Acid – Water – Catalyst TiO2” (150,00 руб.)

0   0
Первый авторGaryntseva
АвторыIrina G., Alexander A., Andrey M., Boris N., Oxana P., Vladimir E.
Страниц15
ID456636
АннотацияThe composition and structure of the solid and soluble products of birch wood deligniёcation by H2O2 in the presence of TiO2 catalyst were studied. The efёcient deligniёcation of wood proceeds at 100 °C and atmospheric pressure. The obtained microcrystalline cellulose (yield 48.2% mass.), has crystallinity index 0.81 and contain 93.7% mass. cellulose, 5.5% mass. hemicelluloses and 0.5% mass. lignin. Soluble products of birch wood peroxide deligniёcation are mainly presented by 4-O-methylglucuronoxylan (84% rel.), monosaccharides and they contain very few aromatic compounds.
УДК547.474:543.8
Composition of Products of Birch Wood Deligniёcation by Hydrogen Peroxide in the Medium “Acetic Acid – Water – Catalyst TiO2” / NataliaV. Garyntseva [и др.] // Журнал Сибирского федерального университета. Химия. Journal of Siberian Federal University/ Chemistry .— 2015 .— №3 .— С. 138-152 .— URL: https://rucont.ru/efd/456636 (дата обращения: 18.05.2024)

Предпросмотр (выдержки из произведения)

Chemistry 3 (2015 8) 450-464 ~ ~ ~ УДК 547.474:543.8 Composition of Products of Birch Wood Delignifi cation by Hydrogen Peroxide in the Medium “Acetic Acid – Water – Catalyst TiO2 ” Natalia V. Garyntseva*a Irina G. Sudakovaa Andrey M. Skripnikova Oxana P. <...> Skaryna Str., Minsk, 220141, Republic of Belarus Received 12.03.2015, received in revised form 15.05.2015, accepted 18.06.2015 The composition and structure of the solid and soluble products of birch wood delignifi cation by H2 O2 in the presence of TiO2 catalyst were studied. <...> The effi cient delignifi cation of wood proceeds at 100 °C and atmospheric pressure. <...> The obtained microcrystalline cellulose (yield 48.2% mass.), has crystallinity index 0.81 and contain 93.7% mass. cellulose, 5.5% mass. hemicelluloses and 0.5% mass. lignin. <...> Soluble products of birch wood peroxide delignifi cation are mainly presented by 4-O-methylglucuronoxylan (84% rel.), monosaccharides and they contain very few aromatic compounds. <...> All rights reserved * Corresponding author E-mail address: garyntseva@icct.ru catalyst, cellulose, soluble # 450 # Natalia V. Garyntseva, Irina G. Sudakova… <...> Состав продуктов делигнификации древесины березы пероксидом водорода в среде «уксусная кислота – вода – катализатор TiO2 » Н.В. Гарынцеваа А.А. <...> , 36 Изучен состав и строение твердых и растворимых продуктов пероксидной делигнификации древесины березы в присутствии катализатора TiO2 . <...> Установлено, что эффективная делигнификация древесины происходит при 100 °С и атмосферном давлении с получением микрокристаллической целлюлозы (выход 48,2 % мас.), с индексом кристалличности 0,81 и содержанием 93,7 % мас. целлюлозы, 5,5 % мас. гемицеллюлоз, 0,5 % мас. лигнина. <...> Растворимые продукты пероксидной делигнификации древесины березы преимущественно представлены 4-О-метил-глюкуроноксиланом (84 % отн.) и моносахаридами и содержат очень мало ароматических соединений. <...> Ключевые слова: древесина березы, делигнификация, пероксид водорода, уксусная кислота <...>